65-75% Ferromolybdenum Description
Ferromolybdenum forms two solid solutions ( and ) and two intermetallic compounds (ε(Fe7Mo6) and σ(FeMo)) in the ratio of 65-75%. Commercial ferromolybdenum contains about 60% Mo, has a melting point of 1800 to 1900 degree and a density of about 9.0 g/cm³.
The Specification Of 65-75% Ferromolybdenum
|
1. Origin |
|||
|
2. Tariff No |
72027000 |
||
|
3. Quality |
65-75 |
||
|
C |
0.1 |
||
|
1.50 |
|||
|
P |
0.05 |
||
|
S |
0.1 |
||
|
0.5 |
|||
|
0.05 |
|||
|
4. Shape |
Lumps in the range of 5/10-50 mm, 90% min. |
||
|
5. Packaging |
Big bags of 1 ton each; Drums of 250 kg |
||
Note: At the request of the consumer ferromolybdenum is produced: grades FMo60(nk) and FMo60 with a mass fraction of S not more than 0.07% and P not more than 0.03%; grade FMo58 with a mass fraction of Si not more than 3.0%; grade FMo55 with a mass fraction of Sn and Sb not more than 0.03% each.
![]()
![]()
A: Our company has a long-term stock of spot, to meet customer requirements.
Populære tags: 65-75% ferromolybdenum, China 65-75% ferromolybdenum manufacturers, suppliers